Honeywell Capran® 996, Heat Stabilized Nylon Film
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Material Notes: Description: Capran® 996 is a blue tinted, heat-stabilized cast film produced from modified nylon resin. Capran® 996 has excellent heat stability and resistance to pinholing. It can be used at temperatures up to 450°F (232°C) for typical cure cycle times. Applications: Capran® 996 is recommended as bagging film for advanced composite fabrication and other high temperature applications where softness and workability are essential. Information provided by Honeywell.
| Available Properties |
- Density
- Thickness
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Tear Strength Test
- Melting Point
- Shrinkage
|
|
|
|
| Property Data |