Honeywell Capran® Oxyshield™ M-OPA (0.60 mil), Monoaxially Oriented, Co-Extruded In-Line Nylon6/Nylon6/Nylon6 Film
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Material Notes: Description: Capran® Oxyshield™ M-OPA (Machine Direction Oriented Polyamide) is a clear, monoaxially oriented, co-extruded in-line nylon6/nylon6/nylon6 film with high mechanical strength and good gas barrier properties for packaging. Information provided by Honeywell.
| Available Properties |
- Density
- Oxygen Transmission Rate
- Thickness
- Surface Tension
- Film Tensile Strength at Yield, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Coefficient of Friction
- Tear Strength Test
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Shrinkage, MD
- Shrinkage, TD
- Haze
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|