BASF Capron® 5233G HS BK-102, 33% Glass-Filled Nylon 66 (Dry)
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Close Analogs: This product is no longer a part of the BASF NAFTA standard product line.
Material Notes: Capron 5233G HS BK-102 is a 35% glass reinforced, heat stabilized, pigmented black nylon 6,6 injection molding compound offering excellent strength, rigidity, stiffness, creep resistance, and dimensional stability. This balance of engineering properties combined with excellent processability makes it ideal in applications replacing metal. It maintains excellent chemical resistance to greases, oils and hydrocarbons. It is also available in natural and pigmented versions. Capron 5233G HS BK-102 is generally recommended for applications such as window locks, valve bodies, door and window hardware, connectors, switch components, relay parts, terminal blocks, power tool components, gears and automotive housings. Data provided by Allied Signal. Processing: Max. water content 0.12%. Product is supplied in sealed containers and drying is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 85°C (185 °F). Is recommended. Drying time is dependent on moisture level. Melt Temperature: 290-315 degC (555-600 degF). Mold Temperature: 80-95 degC (176-203 degF). Injection and Packing Pressure: 35-125 bar (500-1500psi) A mold temperature of 80-95degC (176-203 degF) is recommended, but temperatures of as low as 45 degC (113degF) and as high as 105 degC (221 degF) can be used where applicable. Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off. Back pressure can be utilized to provide uniform melt consistency and reduce trapped air and gas. A maximum of 3.5 bar (50 psi) is recommended to minimize glass fiber breakage. Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing. Surface appearance is directly affected by injection rate.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Viscosity Measurement
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Poissons Ratio
- Dielectric Strength
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Processing Temperature
- Mold Temperature
- Drying Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|