BASF Capron® 8200CQ Blend Nylon 6 (Dry)
Subcategory: Nylon; Thermoplastic; Nylon 6
Close Analogs: This product is no longer a part of the BASF NAFTA standard product line.
Material Notes: Capron 8200CQ Blend is a medium viscosity, nylon 6 injection molding homopolymer possessing the combination of strength, stiffness and toughness properties as well as chemical and abrasion resistance. It is available in natural, heat stabilized and pigmented versions. Capron 8200CQ Blend is generally recommended for applications such as textile components, filter housings, hinges, gears, medical parts, cattle ear tags, wiring devices, plugs, receptacles, gears and connectors. Data provided by Allied Signal. Processing: Max. water content 0.25%. Product is supplied in sealed containers and drying is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 85°C (185 °F). Is recommended. Drying time is dependent on moisture level. Melt Temperature: 240-280 degC (464-536 degF). Mold Temperature: 80-95 degC (176-203 degF). Injection and Packing Pressure: 35-125 bar (500-1500psi) A mold temperature of 80-95 degC (176-203 degF) is recommended, but temperatures of as low as 10 degC (50 degF) can be used where applicable. Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off. Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Viscosity Measurement
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Flexural Yield Strength
- Poissons Ratio
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Drying Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|