BASF Capron® 8202C HS Nylon 6 (Dry)
Subcategory: Nylon; Thermoplastic; Nylon 6
Close Analogs: This product is no longer a part of the BASF NAFTA standard product line.
Material Notes: Capron 8202C HS is a heat stabilized, low viscosity, polyamide 6 injection molding homopolymer possessing a modified crystalline structure for increased property performance and faster cycles. It is also available in non-heat stabilized (Capron 8202C) and/or pigmented versions. Capron 8202C HS is generally recommended for applications such as gears, valves, fittings, insulators, bushings, slides, window hardware, wiring devices, textile components and furniture casters. ASTM Callout PA242. Data provided by Allied Signal. Processing: Max. water content 0.25%. Product is supplied in sealed containers and drying is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 85°C (185 °F). Is recommended. Drying time is dependent on moisture level. Melt Temperature: 240-280 degC (464-536 degF). Mold Temperature: 80-95 degC (176-203 degF). Injection and Packing Pressure: 35-125 bar (500-1500psi) A mold temperature of 80-95 degC (176-203 degF) is recommended, but temperatures of as low as 10 degC (50 degF) can be used where applicable. Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off. Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Viscosity Measurement
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Poissons Ratio
- Coefficient of Friction
- Coefficient of Friction, Static
- Electrical Resistivity
- Dielectric Strength
- Comparative Tracking Index
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Processing Temperature
- Mold Temperature
- Drying Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|