BASF Capron® 8260 HS BK-102, 40% Mineral-Filled Nylon 6 (Conditioned)
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Close Analogs: This product is no longer a part of the BASF NAFTA standard product line.
Material Notes: Capron 8260 HS BK-102 is a heat stabilized, pigmented black, 40% mineral reinforced nylon 6 injection molding resin. It possesses high stiffness, dimensional stability and heat resistance combined with excellent processability including low warp and resistance to sink-mark formation. It maintains its inherent chemical resistance to greases, oils and hydrocarbons. Capron 8260 HS BK-102 is generally recommended for applications such as marine hardware, brackets, fittings, bobbins, office furniture, appliance components, and power tool housings. Data provided by Allied Signal.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Melting Point
- Processing Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|