BASF Capron® 8351 HS BK-102 Impact Modified Nylon 6 (Conditioned)
Subcategory: Nylon; Thermoplastic; Nylon 6
Close Analogs: This product is no longer a part of the BASF NAFTA standard product line.
Material Notes: Capron 8351 HS BK-102 is a heat stabilized, pigmented black type 6 nylon graft copolymer developed for injection molding applications requiring a high level of toughness combined with a moderate flexibility and faster cycles. Excellent thermal and chemical resistance properties provided by the polyamide backbone. It demonstrates the highest impact performance within the Capron copolymer product line while maintaining an excellent balance of strength and stiffness. Excellent chemical resistance to greases, oils and hydrocarbons. Capron 8351 HS Bk-102 is generally recommended for applications such as spray gun and power tool handles, trim clips and fasteners, wall anchors and automotive roof clips rack components. Data provided by Allied Signal. Processing: Max. water content 0.2%. Product is supplied in sealed containers and drying is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 85°C (185 °F). Is recommended. Drying time is dependent on moisture level. Melt Temperature: 240-270 degC (464-518 degF). Mold Temperature: 80-95 degC (176-203 degF). Injection and Packing Pressure: 35-125 bar (500-1500psi) A mold temperature of 80-95 degC (176-203 degF) is recommended, but temperatures of 10-95 degC (50-203 degF) can be used where applicable. Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off. Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melting Point
- Processing Temperature
- Mold Temperature
- Drying Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|