|   BASF Capron® SEG3 H1, 15% Glass-Filled Nylon 6 (Dry)  Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer Close Analogs: This product is no longer a part of the BASF NAFTA standard product line. Material Notes: Capron SEG3 H1 is a 15% glass reinforced nylon 6 injection molding compound exhibiting. It exhibits exceptional surface aesthetics at the slower fill speeds associated with the gas assist injection molding process. It maintains excellent strength, stiffness, high temperature performance and dimensional stability.  Other attributes are: inherent chemical resistance, particularly to greases, oils and hydrocarbons.
 Capron SEG3 H1 is generally recommended for applications such as metal replacements, particularly thinwall parts requiring high flow. Data provided by Allied Signal. Processing: Max. water content 0.16%.  Product is supplied in sealed containers and drying is not required.  If drying becomes necessary, a dehumidifying or desiccant dryer operating at 85°C (185 °F). Is recommended.  Drying time is dependent on moisture level. Melt Temperature: 250-280 degC (482-536 degF).  Mold Temperature:  80-95 degC (176-203 degF).  Injection and Packing Pressure:  35-125 bar (500-1500psi)  This product can be processed over a wide range of mold  temperatures; however, for applications where aesthetics  critical, a mold surface temperature of 80-95 degC (176-203 degF) is required.  Injection pressure controls the filling of the part and should  be applied for 90% of ram travel.  Packing pressure affects  the final part and can be used effectively in controlling  sink marks and shrinkage.  It should be applied and maintained  until the gate area is completely frozen off.    Back pressure can be utilized to provide uniform melt consistency  and reduce trapped air and gas.  A maximum of 3.5 bar (50 psi) is  recommended to minimize glass fiber breakage.  Fast fill rates are recommended to insure uniform melt  delivery to the cavity and prevent premature freezing. Surface  appearance is directly affected by injection rate.   
| | 
    | Available Properties |  
    | Linear Mold ShrinkageTensile Strength, UltimateFlexural ModulusFlexural Yield StrengthMelting PointDeflection Temperature at 0.46 MPa (66 psi)Deflection Temperature at 1.8 MPa (264 psi)Drying Temperature
 | 
 | 
 |  | | 
    | Property Data |  
    | 
    This page displays only the textof a material data sheet.
 
 To see MatWeb's complete data
 sheet for this material (including
 material property data, metal
 compositions, material suppliers,
 etc), please click the button below.
 |  
    |  | 
 | 
 | 
 |