Amity Phenolic Molding ATS 766, Chopped cotton fabric Filler, Compression Molded
Subcategory: Phenolic; Thermoset; Polymer
Material Notes:
Characteristics: High impact strengthGlossy surfaceLow shrinkageGood sliding propertiesColor-BrownMedium flowApplications: Cog wheelsCastor wheelsBush bearingsPulleysWelding rod handlesTextile bobbins etc.Information provided by Amity Thermosets Limited
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength at Break
- Shear Strength
- Izod Impact, Notched
- Mold Temperature
- Injection Pressure
- Cure Time
- Shelf Life
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|