Amity Phenolic Molding ATM 144, Organic Filler, Compression Molded
Subcategory: Phenolic; Thermoset; Polymer
Material Notes:
Characteristics: Good mouldability Good mechanical strengthGood electrical insulationGood surface finishMedium thermal stabilityColor- black, brownSoft/medium flow Applications: Electric control panel parts Small electric meter covers & partsElectric accessories ( superior quality )Glossy handles & knobsToaster & electric appliance partsLamp holderToilet seatsCarbon brush holdersDecor items ( e.g. ash trays )Starter push buttonsSolenoid switch covers ( medium quality ) Kitchen equipment ( eg. mixer, dishwasher, ovens ) fittingsTerminal boards, etc.Information provided by Amity Thermosets Limited
| Available Properties |
- Density
- Apparent Bulk Density
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength at Break
- Shear Strength
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Strength
- Mold Temperature
- Injection Pressure
- Cure Time
- Shelf Life
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|