Amity Phenolic Molding ATO 176, Organic and inorganic Filler, Compression Molded
Subcategory: Phenolic; Thermoset; Polymer
Material Notes:
Characteristics: Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackMedium flow Applications: Heat shields Oven knobs Toaster knobsCoffee machine baseThermal insulationSwitchgear components which ought to withstand heat (200 0C), etc.
Information provided by Amity Thermosets Limited
| Available Properties |
- Density
- Apparent Bulk Density
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength at Break
- Shear Strength
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Strength
- Maximum Service Temperature, Air
- Mold Temperature
- Injection Pressure
- Cure Time
- Shelf Life
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|