Amity Phenolic Molding ATS 132, Organic, inorganic, and graphite Filler, Compression Molded
Subcategory: Phenolic; Thermoset; Polymer
Material Notes:
Characteristics: Self lubricating ( graphite modified )Good glide propertiesGood sealing propertiesMedium or low mechanical strengthUnsuitable for electrical applicationGlossy surfaceThermal conductivityColor-gray Medium flow Applications: SealsSelf lubricating parts / housings , etc.
Information provided by Amity Thermosets Limited
| Available Properties |
- Density
- Apparent Bulk Density
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength at Break
- Shear Strength
- Izod Impact, Notched
- Mold Temperature
- Injection Pressure
- Cure Time
- Shelf Life
|
|
|
|