Amity Phenolic Molding ATS 1612, Nylon, inorganic, and glass Filler, Compression Molded
  Subcategory: Phenolic; Thermoset; Polymer 
Material Notes: 
 Characteristics: High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications: Railway signaling equipment parts Kitchen equipment ( e.g. mixers,   dishwashers ) parts  Components which ought to have good electric insulation in spite of exposure to humid atmosphere, etc.Information provided by Amity Thermosets Limited  
  
  
    | Available Properties | 
   
    
    - Density
 
- Apparent Bulk Density
 
- Water Absorption
 
- Linear Mold Shrinkage
 
- Tensile Strength at Break
 
- Shear Strength
 
- Izod Impact, Notched
 
- Volume Resistivity
 
- Surface Resistance
 
- Dielectric Strength
 
- Mold Temperature
 
- Injection Pressure
 
- Cure Time
 
- Shelf Life
 
 
   |   
   |   
 | 
   | 
  
  
    | Property Data | 
   
    
    This page displays only the text 
    of a material data sheet.
  
    To see MatWeb's complete data 
    sheet for this material (including 
    material property data, metal 
    compositions, material suppliers, 
    etc), please click the button below.  | 
   
    | 
    
     | 
    
   |   
 |   
  
   |