Amity Phenolic Molding ATF 197, Inorganic and glass Filler, Compression Molded

 

Subcategory: Phenolic; Thermoset; Polymer

Material Notes:

Characteristics:

  • Flame retardant
  • Spark resistant
  • Good electrical insulation
  • Heat stability ( 200°C )
  • Good mouldability
  • Low water absorption
  • Low shrinkage
  • Color-black
  • Soft/medium flow
  • Applications:

  • Switchgear components exposed to spark
  • Automotive ( electrical, electronic ) parts
  • Decor items ( ash trays )
  • Superior quality handles & knobs often exposed to flame
  • Automotive lamp caps
  • Moudlings exposed to warm & humid climate
  • Moulding exposed to low intensity flame and spark, etc.
  • Information provided by Amity Thermosets Limited

    Available Properties
    • Density
    • Apparent Bulk Density
    • Water Absorption
    • Linear Mold Shrinkage
    • Tensile Strength at Break
    • Shear Strength
    • Izod Impact, Notched
    • Volume Resistivity
    • Surface Resistance
    • Dielectric Strength
    • Comparative Tracking Index
    • Mold Temperature
    • Injection Pressure
    • Cure Time
    • Shelf Life
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。