Amity Phenolic Molding ATF 197, Inorganic and glass Filler, Compression Molded
Subcategory: Phenolic; Thermoset; Polymer
Material Notes:
Characteristics: Flame retardantSpark resistant Good electrical insulationHeat stability ( 200°C )Good mouldability Low water absorptionLow shrinkageColor-blackSoft/medium flow Applications: Switchgear components exposed to sparkAutomotive ( electrical, electronic ) partsDecor items ( ash trays )Superior quality handles & knobs often exposed to flameAutomotive lamp caps Moudlings exposed to warm & humid climateMoulding exposed to low intensity flame and spark, etc.Information provided by Amity Thermosets Limited
| Available Properties |
- Density
- Apparent Bulk Density
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength at Break
- Shear Strength
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Strength
- Comparative Tracking Index
- Mold Temperature
- Injection Pressure
- Cure Time
- Shelf Life
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|