Anocast Silica-filled Epoxy Polymer Composite
Subcategory: Epoxy; Thermoset; Polymer
Material Notes: Composition is 92% silica and 8% epoxy. The primary application of Anocast is for vibration damping. Features better vibration dampening than metals and natural stone; better thermal stability than metal structures; resistance to corrosive materials and environments; dimensional stability (retention of finished flatness and perpendicularity); ability to embed inserts, rails, plates, recessed pockets and raised bosses; a room temperature casting process; and a finish surface of the casting that is an exact replica of the mold surface. Loss factor is 0.013 at 2696 Hz (Mode 1) and 0.009 at 6622 Hz (Mode 2) - far higher than steel, cast iron, or aluminum. Information provided by Anocast, a Rockwell Automation Business.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Flexural Yield Strength
- Compressive Yield Strength
- Poissons Ratio
- Electrical Resistivity
- Dielectric Constant
- Dielectric Constant, Low Frequency
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|