Advanced Polymer Alloys (APA) Alcryn™ 2165 TR Melt Processible Rubber

 

Subcategory: Elastomer, TPE; Thermoplastic

Material Notes:
The newly introduced 2100 Series grades of Alcryn® offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn®. The new 2100 grades bond to polycarbonate, ABS, polycarbonate/ABS alloys, SAN, ASA, copolyester elastomers and TPUs, as well as both flexible and rigid PVC. The 2100 series

  • is high flow in general plastic processing
  • is designed for injection molding and overmolding
  • is excellent for complex extrusions
  • is excellent for co-extrusions

  • injection molded and overmolded parts
  • soft touch handles and grips on appliance and tool applications
  • automotive interior applications
  • noise and vibration deadening
  • seals and gaskets for automotive insert molding
  • window and door weather stripping (and other complex profile extrusions)
  • coated fabrics and sheet goods
  • wire and cable jackets
  • tubing and hose
  • blow molded parts

Information provided by Advanced Polymer Alloys

Available Properties
  • Specific Gravity
  • Viscosity
  • Hardness, Shore A
  • Tensile Strength @ Break
  • Elongation at Break
  • 100% Modulus
  • Graves Tear Strength
  • Compression Set
  • Tensile Set
  • Processing Temperature
  • Fluid Resistance - Volume Change, % (ASTM D471)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。