Advanced Polymer Alloys (APA) Alcryn 2170 BK Melt Processible Rubber
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes: Alcryn 2100 Series melt-processible rubber (MPR) offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn. The 2100 grades bond to polycarbonate, ABS, polycarbonate/ABS alloys, SAN, ASA, copolyester elastomers and TPUs, as well as both flexible and rigid PVC. Applications: Injection-molded and overmolded partsSoft touch handles and gripsAutomotive interior applicationsSeals and gaskets for automotive insert moldingNoise and vibration deadeningBlow-molded partsTubing and hoseWire and cable jacketsCoated fabrics and sheet goodsWindow and door weatherstrippingInformation provided by Advanced Polymer Alloys
| Available Properties |
- Specific Gravity
- Viscosity
- Hardness, Shore A
- Tensile Strength @ Break
- Elongation at Break
- 100% Modulus
- Graves Tear Strength
- Compression Set
- Tensile Set
- Brittleness Temperature
- Clash Berg Stiffness Temperature
- Processing Temperature
- Fluid Resistance - Volume Change, % (ASTM D471)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|