Advanced Polymer Alloys (APA) Alcryn 2090 BK Melt Processible Rubber

 

Subcategory: Elastomer, TPE; Thermoplastic

Material Notes:
Alcryn melt-processible rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high productivity on thermoplastic processing equipment.

Applications:

  • Window and door weatherstripping (and other complex profile extrusions)
  • Soft handles and grips
  • Molded seals and gaskets
  • Injection-molded and co-injection molded parts
  • Blow-molded parts
  • Tubing and hose
  • Wire and cable jackets
  • Coated fabrics and sheet goods
  • Information provided by Advanced Polymer Alloys

    Available Properties
    • Specific Gravity
    • Viscosity
    • Hardness, Shore A
    • Tensile Strength, Ultimate
    • Elongation at Break
    • Modulus of Elasticity
    • Graves Tear Strength
    • Compression Set
    • Compression Set, Elevated Temperature
    • Tensile Set
    • Clash Berg Stiffness Temperature
    • Processing Temperature
    • Fluid Resistance - Volume Change, % (ASTM D471)
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。