Advanced Polymer Alloys (APA) DuraGrip DGR 6060 NC Thermoplastic Elastomer (TPE)
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes: DuraGrip® DGR 6060NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in injection molding and extrusion processes. DGR 6060NC has an
excellent soft touch feel, will bond to olefinics, is easy to color, and is available in FDA compliant formulations. DuraGrip® is not hygroscopic and under normal conditions does not require drying.Information provided by Advanced Polymer Alloys
| Available Properties |
- Specific Gravity
- Viscosity
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Graves Tear Strength
- Taber Abrasion, mg/1000 Cycles
- Compression Set
- Compression Set, Elevated Temperature
- Tensile Set
- Brittleness Temperature
- Processing Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Injection Pressure
- Cycle Time - Injection
- Screw Speed
- Cure Time
- Fluid Resistance - Volume Change, % (ASTM D471)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|