Advanced Polymer Alloys (APA) DuraGrip DGR 6080 NC/BK Thermoplastic Elastomer (TPE)
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes: DuraGrip® DGR 6080NC/BK are designed to be a general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR
6080NC/BK have excellent soft touch feel, will bond to olefinics, are easy to color, and are available in FDA compliant formulations. DuraGrip® is not hygroscopic and under normal
conditions does not require drying.Information provided by Advanced Polymer Alloys
| Available Properties |
- Specific Gravity
- Viscosity
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Graves Tear Strength
- Taber Abrasion, mg/1000 Cycles
- Compression Set
- Compression Set, Elevated Temperature
- Tensile Set
- Brittleness Temperature
- Processing Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Injection Pressure
- Cycle Time - Injection
- Screw Speed
- Cure Time
- Fluid Resistance - Volume Change, % (ASTM D471)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|