Advanced Polymer Alloys (APA) DuraGrip DGR 6140 UT Thermoplastic Elastomer (TPE)
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes: DuraGrip® DGR 6140UT is an unfilled translucent Thermoplastic Elastomer (TPE). It is designed to process easily in injection molding and extrusion applications. DuraGrip® TPE
features excellent soft touch feel, will bond to ABS, PC, Isoplast, clear copolyester and acrylics, and because it is translucent it is easily colored with a minimum of concentrate. DuraGrip® TPE is not hygroscopic and under normal conditions does not require drying.Information provided by Advanced Polymer Alloys
| Available Properties |
- Specific Gravity
- Viscosity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|