Advanced Polymer Alloys (APA) DuraGrip DGR 6170 NC Thermoplastic Elastomer (TPE)
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes: DuraGrip® DGR 6170 is offered in an NC (colorable) version, and is designed to chemically bond to a wide variety of thermoplastic substrates including ABS, PC, Nylon 6,
Nylon 6/6, glass filled Nylon, ASA, PC/ABS alloys, PBT, and PC/PBT alloys. It is easy to use in injection molding and extrusion processes. DGR 6170NC has excellent elastomeric properties and soft touch feel. DuraGrip® bonding grades are hygroscopic, and for best results drying is recommended prior to use.Information provided by Advanced Polymer Alloys
| Available Properties |
- Specific Gravity
- Viscosity
- Hardness, Shore A
- Tensile Strength @ Break
- Elongation at Break
- 100% Modulus
- Graves Tear Strength
- Compression Set
- Tensile Set
- Brittleness Temperature
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|