Advanced Polymer Alloys (APA) DuraGrip™ 6070 BK Thermoplastic Elastomer
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes: DuraGrip® DGR 6070NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in the injection molding process. DGR 6070NC has an excellent soft touch feel, will bond to olefinics, is easy to color, and is available in FDA compliant formulations. DuraGrip® is not hygroscopic and under normal conditions does not require drying.Information provided by Advanced Polymer Alloys
| Available Properties |
- Specific Gravity
- Viscosity
- Hardness, Shore A
- Tensile Strength @ Break
- Elongation at Break
- 100% Modulus
- 300% Modulus
- Graves Tear Strength
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|