Advanced Polymer Alloys (APA) DuraGrip™ 6140 TR Thermoplastic Elastomer
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes: DuraGrip® DGR6140TR is a translucent thermoplastic elastomer formulated for excellent elastic properties and enhanced adhesion to various engineered thermoplastics using insert molding, co-injection molding and co-extrusion processes. 6140TR bonds tenaciously to polycarbonate, polycarbonate alloys, ABS, ASA, acrylics, and cellulosic materials. It will also bond to various nylons and PET. DuraGrip 6140TR is hygroscopic and drying is recommended at 150F for 3 to 4 hours to ensure optimum aesthetics, properties and adhesion.Information provided by Advanced Polymer Alloys
| Available Properties |
- Specific Gravity
- Viscosity
- Melt Index of Compound
- Hardness, Shore A
- Tensile Strength @ Break
- Elongation at Break
- 100% Modulus
- 300% Modulus
- Graves Tear Strength
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|