Applied Composites Corporation #8022 Polyester SMC
Subcategory: Polyester, TS; Thermoset; Polymer
Key Words: Sheet Molding Compound
Material Notes: Industry Application: Construction Product Application: Water Treatment Distinct Features: Ideal for Buried Applications, Construction, High Corrosion Resistance in Waste Water Treatment, Dimensional Stability Information provided by Applied Composites Corporation.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Barcol
- Tensile Strength, Ultimate
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Izod Impact, Unnotched @ 23°C
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|