Aptek 2712-A/B Very low stress silicone adhesive
Subcategory: Silicone; Adhesive; Thermoset
Material Notes: Very low stress silicone adhesive; -110ºC to 260ºC operating range; Low outgassing/space grade APTEK 2712-A/B is a two component, white, very soft, thixotropic, electrically insulative, silicone adhesive displaying excellent flow temperature flexibility and unusually high physical strength properties. APTEK 2712-A/B has been designed to fully cure at room temperature and can be accelerated with a brief low temperature cure. This 100% solid system has been manufactured with highly pure resins to minimize the occurrence of ionic contamination without outgassing during cure or service. Very flexible/low modulus over wide temperature range to absorb stress build-up during thermal cycling; Convenient 1:1 PBW or PBV mix ratio for easy handling-ideal for cartridge dispensers/repair kits; Very good adhesion to various substrates when used in conjunction with APTEK P-107 primer; Long work life, short cure cycle options for improved productivity on large area bonding applications. APTEK 2712A is a white silica-filled silicone resin blend. APTEK 2712B is a translucent silica-filled silicone resin blend. Information provided by Aptek Laboratories, Inc.
| Available Properties |
- Density
- Outgassing - Total Mass Loss
- Collected Volatile Condensable Material
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Shear Strength
- Tear Strength
- Volume Resistivity
- Dielectric Strength
- CTE, linear 20°C
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Glass Temperature
- Flash Point
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|