Aptek 6513-A/B Versatile, fast set adhesive
Subcategory: Adhesive; Thermoset
Material Notes: APTEK 6513-A/B is a hazy clear, two component, general purpose, semi-rigid, paste adhesive for bonding to steel, aluminum, wood, concrete, glass, ceramics, bras, and a variety of plastics. It is specifically designed to fully cure at room temperature or can be accelerated with moderate heat. Fast set-Reaches 90% of properties in 24 hours at 25ºC(77ºF); Available in convenient tube kits or dual cartridge mixer/dispensers for field repair applications; Smooth thixotropic consistency for easy handling and minimum sag; Contains no diluents or solvents to minimize formation of voids during cure; Capable of curing at ambient temperatures as low as -7ºC(20ºF) Information provided by Aptek Laboratories, Inc.
| Available Properties |
- Density
- Hardness, Shore D
- Shear Strength
- Flash Point
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|