Aptek 2214-A/B Low modulus urethane ESD coating/adhesive
Subcategory: Adhesive; Polyurethane, TS; Thermoset
Material Notes: Space Grade, Low modulus urethane ESD coating/adhesive APTEK is a carbon-filled, thixotropic, two component, electrically conductive, flexible urethane coating/adhesive designed to dissipate an electrostatic charge. This low-outgassing system provides a combination of high flexibility and good tensile strength/elongation characteristics. Capable of full cure at RT for application where heat cure is not desired or possible; Exceeds NASA outgassing requirements for space applications; Non-TDI based for safety; Excellent version resistance for good physical stability under high heat and humidity environments; Tg below -60ºC for excellent low temperature cycling, storage and performance; Excellent substrate adhesion; superior to silicones; Available in pre-measured kits to minimize handling APTEK 2214A is a black carbon-filled polyol resin. APTEK 2214B is a pale yellow organic isocyanate. Information provided by Aptek Laboratories, Inc.
| Available Properties |
- Density
- Viscosity
- Outgassing - Total Mass Loss
- Collected Volatile Condensable Material
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Surface Resistance
- Glass Temperature
- Flash Point
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|