Aptek 2313-PMF Hybrid Epoxy Adhesive
Subcategory: Epoxy; Adhesive; Thermoset
Material Notes: Snap-cure, silver-filled; long pot-life/stable viscosity-excellent for robotics. Thermal shock resistant. Production-oriented, snap-cure technology for surface mount applications-allows cure during solder reflow operation. High thixotropy/"tack" strength-holds components with minimal "Z" axis movement during cure. Stable viscosity for over 4 hours at RT-ideal for robotics. Low Tg (<-50°C) for excellent low temperature cycling and performance with minimal stress. Excellent substrate adhesion; superior to silicones: no primer required. Information provided by Aptek Laboratories, Inc.
| Available Properties |
- Density
- Shear Strength
- Volume Resistivity
- Thermal Conductivity
- Glass Temperature
- Flash Point
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|