Aptek 2710A/B Low modulus silicone adhesive

 

Subcategory: Silicone; Adhesive; Thermoset

Material Notes:
Low modulus silicone adhesive; -110ºC to 260ºC operating range; Low outgassing/space grade; Electrostatically Discharging (ESD)
APTEK 2710-A/B is a two component, black, low modulus, thixotropic, silicone adhesive displaying very low temperature flexibility and good physical strength properties. APTEK 2710-A/B has been designed to fully cure at room temperature and can be accelerated with a brief low temperature cure. This 100% solid system has been manufactured with highly pure resins to minimize the occurrence of ionic contamination without outgassing during cure or service.

Utilizes silicone technology providing very low Tg for excellent low temperature performance; Convenient 1:1 PBW or PBV mix ration for easy handling - ideal for cartridge dispensers/repair kits; Very flexible/low modulus over wide temperature range to absorb stress build-up during thermal cycling; Very good adhesion to various substrates when used in conjunction with APTEK P-105 primer

Information provided by Aptek Laboratories, Inc.

Available Properties
  • Density
  • Outgassing - Total Mass Loss
  • Collected Volatile Condensable Material
  • Hardness, Shore A
  • Shear Strength
  • Volume Resistivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Temperature
  • Flash Point
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。