Aptek 6500-PMF Electrically conductive epoxy adhesive
Subcategory: Epoxy; Adhesive; Thermoset
Material Notes: High purity, low outgassing, electrically conductive adhesive APTEK 6500-PMF is a one component, pre-mixed frozen, 100% solid, silver-filled epoxy adhesive specifically designed for microelectronic die attach applications High purity resin system for minimum level of ionic contamination to prevent corrosion problems; High cross-link density to maintain stability and minimize outgassing during operational life even in high-vacuum environments and sealed packages; Smooth thixotropic consistency for machine stamping applications; Viscosity can be factory controlled for screening or dispensing applications; Contains no diluents or solvents to minimize formation of voids during cure Information provided by Aptek Laboratories, Inc.
| Available Properties |
- Density
- Viscosity
- Outgassing - Total Mass Loss
- Collected Volatile Condensable Material
- Hardness, Shore D
- Shear Strength
- Volume Resistivity
- CTE, linear 20°C
- Glass Temperature
- Flash Point
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|