Aptek 1303 B/C/B Thermally conductive urethane film adhesive

 

Subcategory: Polyurethane, TS; Thermoset

Material Notes:
Thermally conductive, electrically insulating hybrid urethane film adhesive
APTEK 1303B/C/B is a low modulus, flexible, void free, electrically insulating hybrid urethane film adhesive designed to bond dissimilar components and substrates. This B/C/B system is designed to manage stresses developed from mismatches of thermal expansion coefficients during temperature cycling as well as to dissipate heat generated from components and circuitry. APTEK 1303 B/C/B technology incorporates a partially-cured (B-staged) adhesive on both faces of a fully-cured (C-staged) ultra low modulus film. APTEK 1303 B/C/B film is a 100% solids, thermoset polymer, which will not outgas, while in place and is suitable for high vacuum environments. The film exhibits outstanding reversion resistance and physical stability under long-term aging of high humidity and heat.

Low modulus/high elongation for minimum stress buildup under components; Low Tg-remains flexible to -75°C; Exceeds NASA outgassing requirements for high vacuum environments; Typical film thickness, .006" to .012". Customer thicknesses available; Available in sheet or die-cut forms; Low tack adhesive layer allows for easy placement and, if needed, repositioning on assemblies

Information provided by Aptek Laboratories, Inc.

Available Properties
  • Density
  • Moisture Absorption at Equilibrium
  • Outgassing - Total Mass Loss
  • Collected Volatile Condensable Material
  • Elongation at Break
  • Tensile Modulus
  • Shear Strength
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear 20°C
  • Thermal Conductivity
  • Glass Temperature
  • Processing Temperature
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。