Aptek UVISTAKE 7205LM-PMF UV Curing, Low Outgassing, Urethane staking compound
Subcategory: Polyurethane, TS; Thermoset
Material Notes: UVISTAKE 7205LM-PMF is a 100% solids, thixotropic, one component, premixed frozen, electrically insulating, urethane system designed for the attachment and staking of electrical/electronic components mounted on printed circuit boards. This system provides an excellent combination of flexibility and strength for demanding applications where toughness is required for the management of thermomechanical stresses. UVISTAKE 7205LM-PMF will become tack free when exposed to the proper UV light radiation. The staking compound will fully post cure in exposed and shaded areas in 14 days at 25ºC and 50% relative humidity, as an alternative, the post cure for the staking compound in both exposed and shaded areas may be accelerated with low to moderate heat. Multicure mechanism for complete cure in shaded areas underneath components; Good flexibility for reduced stress in the encapsulation of sensitive glass-bodied components; Meets NASA condensable volatile requirements for high vacuum environments; Highly reversion resistant for good physical stability under high heat and humidity environments; Excellent adhesion to plastic/metal components and substrates; More rigid version (95A) available as UVISTAKE 7205-PMF; Packaged in syringes for convenient dispensing; No TDI, no toxic solvents, no free acrylic acid for safety Information provided by Aptek Laboratories, Inc.
| Available Properties |
- Density
- Outgassing - Total Mass Loss
- Collected Volatile Condensable Material
- Hardness, Shore A
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- CTE, linear 20°C
- Glass Temperature
- Flash Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|