Aptek UVISTAKE 7206 UV Curing, Urethane staking compound

 

Subcategory: Polyurethane, TS; Thermoset

Material Notes:
UVISTAKE 7206 is a 100% solid, thixotropic, one component, premixed frozen, electrically insulating, urethane system designed for the attachment and staking of electrical/electronic components mounted on printed circuit boards. This system provides an excellent combination of flexibility and strength for demanding applications where toughness is required for the management of the thermomechanical stresses. UVISTAKE 7206 will become tack free when exposed to the proper UV light radiation.

Good flexibility for reduced stress in the encapsulation of sensitive glass-bodied components; Highly reversion resistant for good physical stability under high heat and humidity environments; Excellent adhesion to plastic/metal components and substrates; No TDI, no toxic solvents, no free acrylic acid for safety

Information provided by Aptek Laboratories, Inc.

Available Properties
  • Density
  • Hardness, Shore D
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Glass Temperature
  • Flash Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。