Aptek 2506-A/B Room temperature curing, low modulus urethane conformal coating
Subcategory: Polyurethane, TS; Thermoset
Material Notes: Room temperature curing, low modulus urethane conformal coating APTEK 2506-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the encapsulation and protection of electrical/electronic components mounted on printed circuit boards. Capable of curing at RT, rapid cure with low/moderate heat cycle; Non-TDI based for safety; Excellent reversion resistance for good physical stability under high heat and humidity environments; Tg below -55ºC for excellent low temperature cycling, storage and performance; Excellent substrate adhesion; superior to silicones; Fluoresces under black-light (UV) APTEK 2506-A is a blue unfilled polyol resin. APTEK 2506-B is a amber colored organic isocyanate which make cause severe eye and skin irritation with direct contact.. Information provided by Aptek Laboratories, Inc.
| Available Properties |
- Density
- Viscosity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Glass Temperature
- Flash Point
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|