Aptek 7504LM-PMF UV Urethane Coating/Encapsulant
Subcategory: Polyurethane, TS; Thermoset
Material Notes: UV-cured,100% solids version of UVIKOTE 7503 LM-PMF. Castable/brushable viscosity for higher coating build-up. QPL listed on MIL-I-46058C, types UR an AR. Information provided by Aptek Laboratories, Inc.
| Available Properties |
- Density
- Viscosity
- Outgassing - Total Mass Loss
- Collected Volatile Condensable Material
- Hardness, Shore A
- Modulus of Elasticity
- Volume Resistivity
- Insulation Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Glass Temperature
- Flash Point
- Color
|
|
|
|