|   Aptek 6103-A/B Epoxy Encapsulant  Subcategory: Epoxy; Thermoset Material Notes: Optoelectronic grade, reddish black encapsulant for IR LED discreets. Transparent to IR light while blocking out visible light.
 Part A is deep red. Part B is clear to pale yellow. Information provided by Aptek Laboratories, Inc. 
| | 
    | Available Properties |  
    | DensityBrookfield ViscosityHardness, Shore DVolume ResistivityDielectric ConstantDissipation FactorCTE, linear 20°CGlass TemperatureFlash PointProcessing Temperature
 | 
 | 
 |  | | 
    | Property Data |  
    | 
    This page displays only the textof a material data sheet.
 
 To see MatWeb's complete data
 sheet for this material (including
 material property data, metal
 compositions, material suppliers,
 etc), please click the button below.
 |  
    |  | 
 | 
 | 
 |