Aptek 6550-A/B Epoxy Encapsulant
Subcategory: Epoxy; Thermoset
Material Notes: High thermal conductivity, microelectronic grade blob-top encapsulant. Ultra high purity. Excellent heat and moisture protection for sensitive chips/circuitry. Premixed frozen syringes available for robotic dispensers. Part A is black. Part B is white. Information provided by Aptek Laboratories, Inc.
| Available Properties |
- Viscosity
- Ionic Impurities - Na (Sodium)
- Ionic Impurities - K (Potassium)
- Ionic Impurities - Cl (Chloride)
- Hardness, Shore D
- Shear Strength
- Volume Resistivity
- CTE, linear 20°C
- Thermal Conductivity
- Glass Temperature
- Flash Point
|
|
|
|