Reltek LLC BONDiT™ B-481 Adhesive, Sealant & Coating System

 

Subcategory: Adhesive; Thermoset; Polymer

Key Words: Epoxy Adhesive, Sealant

Material Notes:
Key Properties:

  • High strength and toughness with excellent thermal stability to 400°F.
  • Outstanding chemical resistance.
  • Excellent electrical, and mechanical properties.
  • Ease of use.

Applications: Encapsule sensitive instrumentation for chemical isolation, outstanding moisture resistance, ruggedness and flexibility. Suitable for clean room use and direct contact with semiconductors. Very easy to use and very clean two-part system. Superior for coating in marine applications and other harsh environments. Tough, high strength, chemically resistant non-blush clear coating with medium gloss finish. Bonds to most substrates. Can be applied to oily surfaces. Ambient 24 hour or accelerated thermal cure.

Available Properties
  • Water Absorption
  • Viscosity
  • Tensile Strength, Ultimate
  • Tensile Strength @ Break
  • Tensile Strength @ Yield
  • Elongation at Break
  • Elongation at Yield
  • Tangent Modulus
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Pot Life
  • Chemical & Moisture Resistance
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。