Reltek LLC BONDiT™ B-4682 Adhesive, Sealant & Coating System
Subcategory: Adhesive; Thermoset; Polymer
Key Words: Epoxy Adhesive, Sealant
Material Notes: Key Properties: Excellent adhesion to low surface energy plastics without primer or surface preparation.Applications: High flexibility, 300% elongation, emphasizing high tack for un-abraded substrates and plastic films. Excellent for water and oil sealing. Can be applied to oily surfaces. Ambient or thermal cure. May be catalyzed for fast set time.
| Available Properties |
- Tensile Strength @ Break
- Elongation at Break
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Cure Time
- Chemical & Moisture Resistance
|
|
|
|