Aquabond Technologies ABS-55 Water Soluble Adhesive and Bonding Thermoplastic

 

Subcategory: Adhesive; Thermoplastic; Polymer

Material Notes:
Description: Aquabond's water soluble thermoplastic is designed for temporary mounting of hard materials for slicing, dicing, grinding, lapping and polishing and comes in 3 different bonding temperatures that can be purchased in either stick or bulk form. All products are virtually insoluble in cold or cool water, thus providing a strong bond in the presence of aqueous cutting lubricants and coolants.

All Aquabond thermoplastic adhesives when submerged in HOT water will go to solution and not return. The use of Aquaclean 900 and ultrasonic or air agitation greatly speeds debonding and aids in producing very clean finished parts. As long as the work piece is non- hazardous, and you already have the proper approvals, the solution can be poured down the drain.

All Aquabond thermoplastic temporary adhesives come in either 100 gram bulk ingots or in 45 gram 5/8 inch diameter sticks for easy application.

Aquabond 55 has the lowest melting and bonding temperature and is generally used for lapping, backgrinding, wafer bonding and wafer thinning. It puddles quickly and can spread as thin as four (4) microns.

Information provided by Aquabond Technologies.

Available Properties
  • Specific Gravity
  • Solubility
  • Viscosity
  • Penetration
  • Melting Point
  • Boiling Point
  • Softening Point
  • Flash Point
  • Processing Temperature
  • Melt Temperature
  • Cure Time
  • Color
  • Debond/Cleanup
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。