Aremco Aremco-Bond™ 568 Conductive Epoxy Adhesive
Subcategory: Epoxy; Adhesive; Thermoset
Material Notes: Thermally conductive, aluminum-filled, 1:1 epoxy paste. Excellent mechanical strength to 400 ºF (205 °C). Data provided by the manufacturer, Aremco Products, Inc. Aremco Products, Inc. makes no warranty express or implied concerning the use of these products. The user assumes all risk of use or handling whether or not in accordance with directions or suggestions, or used singly or in combination with other products.
| Available Properties |
- Density
- Viscosity Measurement
- Electrical Resistivity
- CTE, linear 20°C
- Thermal Conductivity
|
|
|
|