Aremco Aremco-Bond™ 860 Conductive Epoxy Adhesive
Subcategory: Epoxy; Adhesive; Thermoset
Material Notes: Thermally conductive, aluminum nitride filled, 1:1 epoxy paste. Exceptional mechanical and thermal properties to 400 ºF (205 °C). Data provided by the manufacturer, Aremco Products, Inc. Aremco Products, Inc. makes no warranty express or implied concerning the use of these products. The user assumes all risk of use or handling whether or not in accordance with directions or suggestions, or used singly or in combination with other products.
| Available Properties |
- Density
- Viscosity Measurement
- Shear Strength
- Electrical Resistivity
- Dielectric Strength
- CTE, linear 20°C
- Thermal Conductivity
- Pot Life
|
|
|
|