Aremco Aremco-Bond™ 597 Conductive Epoxy Adhesive
Subcategory: Epoxy; Adhesive; Thermoset
Material Notes: Electrically and thermally conductive, silver-filled, one-part paste. Inorganic system for adhesive (597A) & coating (597C) applications to 1200 ºF (650 °C). Data provided by the manufacturer, Aremco Products, Inc. Aremco Products, Inc. makes no warranty express or implied concerning the use of these products. The user assumes all risk of use or handling whether or not in accordance with directions or suggestions, or used singly or in combination with other products.
| Available Properties |
- Density
- Viscosity
- Shear Strength
- Electrical Resistivity
- Dielectric Strength
- CTE, linear 20°C
- Thermal Conductivity
- Pot Life
|
|
|
|