AREMCO Pyro-Duct™ 598-A Electrically & Thermally Conductive Materials, Nickel Filled
Subcategory: Epoxy; Adhesive; Thermoset
Material Notes: Electrically and Thermally conductive, Nickel-Filled, One Part System. Inorganic System for Adhesive (-A) & Coating (-C) Applications to 1000 °F.Information provided by AREMCO
| Available Properties |
- Specific Gravity
- Viscosity
- Volume Resistivity
- CTE, linear 68°F
- Thermal Conductivity
- Maximum Service Temperature, Air
- Cure Time
- Chemical Resistance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|