AREMCO Aremco-Seal™ High Temperature Specialty Coatings 4030 Silicone, Ceramic Filled
Subcategory: Silicone; Adhesive
Material Notes: Hi-temp silicone sealer which prevents dusting of fibrous insulation materials to 1100 ºF. This advanced sealer is used in critical oven and furnace applications in the automotive, electronics and heat treating industries. For alternative colors, refer to Technical Bulletin A6, Corr-Paint™ CP40XX products.Information provided by AREMCO
| Available Properties |
- Specific Gravity
- Solids Content
- Volatile Organic Compounds (VOC) Content
- Viscosity
- Thickness
- Storage Temperature
- Maximum Service Temperature, Air
- Flash Point
- Processing Temperature
- Dry Time
- Cure Time
- Shelf Life
- Dry Film Coverage ft2/gal
- Thinner
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|