AREMCO Pyro-Tape™ High Temperature Tape 682-ER Single layer polyimide film with silicone adhesive
Subcategory: Adhesive; Tape
Material Notes: Applications Features - Electrical insulation for process instrumentation, wiring and harnesses.
- RF induction coil insulation.
- Transformer, terminal and connector insulation.
- Masking gold fingers for printed circuit board wave soldering.
Information provided by AREMCO
| Available Properties |
- Thickness
- Tensile Strength @ Break
- Adhesive Bond Strength
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Maximum Service Temperature, Air
|
|
|
|