|   Arkema Group Orevac® 18732 Maleic Anhydride modified Polypropylene  Subcategory: Polypropylene; Thermoplastic Material Notes: Orevac® 18732 resin is a maleic anhydride modified polypropylene designed for the 3 layer external pipe coating.  It provides outstanding adhesion between the epoxy primer layer and polyethylene topcoat layer.
 Information provided by Arkema Group 
| | 
    | Available Properties |  
    | DensityMelt FlowHardness, Shore DTensile Strength at BreakElongation at BreakMelting PointVicat Softening Point
 | 
 | 
 |  | | 