Arkema Group Orevac® C306 Maleic Anhydride modified LLDPE
Subcategory: Polyethylene; Thermoplastic; LLDPE
Material Notes: Orevac® C306 resin is a maleic anhydride modified LLDPE designed for the coextrusion of multilayer barrier structures providing outstanding adhesion between the layers. Orevac® C306 is characterized by a high level of maleic anhydride. It can be used as is or diluted with polyethylene.Information provided by Arkema Group
| Available Properties |
- Density
- Melt Flow
- Melting Point
|
|
|
|